1075HICARB 1/4 X 2 X  18 1075HICARB 1/4 X 2 X 18

Our 1075 is cold rolled and annealed. This material is perfect for forging, blades, tools and other parts. Very easy to work.
HEAT TREATMENT Bring to 1450°-1475°F, then quench immediately, holding at a non crucial point such as the back of the blade or handle area. Temper between 400°-600°F,
depending upon the desired hardness. Typical chemistry C .70-.80 Mn 0.4-0.7 P .04 Max S .05 Max

Price: $14.65
1075HICARB 1/4 X 4 X  18 1075HICARB 1/4 X 4 X 18

Our 1075 is cold rolled and annealed. This material is perfect for forging, blades, tools and other parts. Very easy to work.
HEAT TREATMENT Bring to 1450°-1475°F, then quench immediately, holding at a non crucial point such as the back of the blade or handle area. Temper between 400°-600°F,
depending upon the desired hardness. Typical chemistry C .70-.80 Mn 0.4-0.7 P .04 Max S .05 Max

Price: $28.30
1075HICARB 1/4 X 2 X 36 1075HICARB 1/4 X 2 X 36

Our 1075 is cold rolled and annealed with a bright finish. This material is perfect for forging, blades, tools and other parts. Very easy to work.
HEAT TREATMENT Bring to 1450°-1475°F, then quench immediately, holding at a non crucial point such as the back of the blade or handle area. Temper between 400°-600°F, depending upon the desired hardness.
Typical chemistry C .90/1.04, Mn .60/.90.

Price: $29.35
1075HICARB 1/4 X 4 X 36 1075HICARB 1/4 X 4 X 36

Our 1075 is cold rolled and annealed with a bright finish. This material is perfect for forging, blades, tools and other parts. Very easy to work. HEAT TREATMENT Bring to 1450°-1475°F, then quench immediately, holding at a non crucial point such as the back of the blade or handle area. Temper between 400°-600°F, depending upon the desired hardness. Typical chemistry C .90/1.04, Mn .60/.90.

Price: $57.70
   
 